| Possible Causes |
Solutions |
| Inherent softness or high friability of core |
Improve mechanical strength of core by increasing compaction force, modifying core formulation or changing process by which core is produced (e.g. use granulation process instead of direct compression |
| Excessive pan speed in coating process |
Reduce pan speed |
| Spray rate too low |
Increase spray rate |
| Low solids content of spray solution |
Select OPADRY II formulation with high solids content |
| Premature swelling of hydrophilic super disintegrant in formulation |
Replace super disintegrant with less hydrophilic disintegrant like STARCH 1500 |